WO2023237231 - PROCESS AND SYSTEM FOR THE CALCINATION OF GYPSUM

National phase entry:
Publication Number WO/2023/237231
Publication Date 14.12.2023
International Application No. PCT/EP2023/025273
International Filing Date 07.06.2023
Title [English] PROCESS AND SYSTEM FOR THE CALCINATION OF GYPSUM [French] PROCÉDÉ ET SYSTÈME DE CALCINATION DE GYPSE
Applicants ** KNAUF GIPS KG Am Bahnhof 7 97346 Iphofen, DE
Inventors ** BAESE, Rauno c/o Knauf Gips KG Am Bahnhof 7 97346 Iphofen, DE GEIGER, Raphael c/o Knauf Gips KG Am Bahnhof 7 97346 Iphofen, DE
Priority Data 22000152.3  08.06.2022  EP
Application details
International Searching Authority
Translation

Recalculate

* The data is based on automatic recognition. Please verify and amend if necessary.

** IP-Coster compiles data from publicly available sources. If this data includes your personal information, you can contact us to request its removal.

Quotation for National Phase entry

Country Stages Total
China Filing 1165
EPO Filing, Examination 5852
Japan Filing 578
South Korea Filing 578
USA Filing, Examination 2635
MasterCard Visa
Total: 10808
The term for entry into the National Phase has expired. This quotation is for informational purposes only.

Abstract [English] The present invention concerns a process for the calcination of raw gypsum in a heatable extruder, wherein the raw gypsum is feed into the extruder and heated to a temperature of from 150°C to 350°C to thereby convert the raw gypsum to calcined gypsum with a content of calcium hemihydrate of at least 50 wt.-%. By using a heatable extruder for the calcination, calcined gypsum with a high content of calcium sulphate hemihydrate and low residual amounts of the respective dihydrate and anhydrite can be obtained. The present invention further concerns a system, which is adapted to such preparation of calcined gypsum and comprises an appropriate heatable extruder and the use of a heatable extruder for the calcination of raw gypsum. [French] La présente invention concerne un procédé de calcination de gypse brut dans une extrudeuse pouvant être chauffée, le gypse brut étant introduit dans l'extrudeuse et chauffé à une température de 150 à 350 °C pour convertir ainsi le gypse brut en gypse calciné avec une teneur en hémihydrate de calcium d'au moins 50 % en poids. L'utilisation dans la calcination d'une extrudeuse pouvant être chauffée permet d'obtenir du gypse calciné doté d'une teneur élevée en hémihydrate de sulfate de calcium et de faibles quantités résiduelles de dihydrate et d'anhydrite respectifs. La présente invention concerne également un système adapté à une telle préparation de gypse calciné et comprenant une extrudeuse appropriée pouvant être chauffée, ainsi que l'utilisation dans la calcination de gypse brut d'une extrudeuse pouvant être chauffée.